Xiong X, Xu K, Du Q, Zeng X, Xiao Y, Yang H, Li H. Effects of Temperature and Solvent on the Solid-State Transformations of Pranlukast During Mechanical Milling.
J Pharm Sci 2017;
106:1680-1687. [PMID:
28249805 DOI:
10.1016/j.xphs.2017.02.020]
[Citation(s) in RCA: 5] [Impact Index Per Article: 0.7] [Reference Citation Analysis] [Abstract] [Key Words] [Track Full Text] [Journal Information] [Subscribe] [Scholar Register] [Received: 11/27/2016] [Revised: 02/03/2017] [Accepted: 02/13/2017] [Indexed: 11/16/2022]
Abstract
Four solid forms of pranlukast (PRS) were obtained during mechanical milling including neat milling (NM) and solvent-drop milling (SDM), which were characterized by various analytical techniques. The effect of milling conditions including 3 milling temperatures and 6 assist solvents on the solid-state transformations of commercial PRS (PRS HH) was systemically investigated. Milling temperature significantly influenced the NM process. A low milling temperature (5°C) led to a complete amorphization of PRS HH, whereas higher milling temperatures (15°C and 30°C) only induced a partial amorphization. The milling at 5°C was proven to be a progressive amorphization process, and the amorphous material showed an increasing stability with prolonged milling time. Amorphous PRS can stay stable under low temperature and relative humidity conditions and showed significantly higher solubilities and faster dissolution rates in both water and pH 6.8 phosphate buffer solution. A total of 6 solvents were used in the SDM experiments. N,N-dimethylformamide and dimethyl sulfoxide should be avoided in the manufacturing process of PRS because corresponding solvates of PRS can be easily generated by SDM of PRS HH with short milling time and small amount of solvents.
Collapse