Auychai P, Khumtrakoon N, Jitongart C, Daomanee P, Laiteerapong A. Bond Strength and Microleakage of a Novel Glass Ionomer Cement Containing Silver Diamine Fluoride.
Eur J Dent 2021;
16:606-611. [PMID:
34921382 PMCID:
PMC9507574 DOI:
10.1055/s-0041-1736329]
[Citation(s) in RCA: 0] [Impact Index Per Article: 0] [Reference Citation Analysis] [What about the content of this article? (0)] [Affiliation(s)] [Abstract] [Track Full Text] [Figures] [Journal Information] [Subscribe] [Scholar Register] [Indexed: 11/17/2022] Open
Abstract
Objectives
To investigate the shear bond strength and microleakage of glass ionomer cement (GIC) containing silver diamine fluoride (SDF).
Materials and Methods
Sound human permanent premolars were divided into the following three groups: 1) GIC (Fuji IX), 2) GICSDF-S: GIC + SDF (Saforide), and 3) GICSDF-T: GIC + SDF (Topamine). Shear bond strength (
n
= 14/group) was measured using a universal testing machine and compared between groups (one-way ANOVA and Tukey HSD,
p
< 0.05). Microleakage (
n
= 15/group) at enamel and dentin margins was scored using a stereomicroscope (10x) and compared between groups (Chi-square,
p
< 0.05).
Results
There were significant differences in shear bond strength between the GIC and GICSDF-S groups and between the GIC and GICSDF-T groups. The GIC group had the lowest shear bond strength among the groups; however, there was no significant difference between the GICSDF-S and GICSDF-T groups. The microleakage test results were not significantly different between groups at the enamel margin or dentin margins. Although the GIC group demonstrated a higher dye penetration score at the enamel and dentin margins, the difference was not significant.
Conclusions
Within the limitations of this study, we conclude that incorporating SDF into GIC results in higher shear bond strength while not increasing microleakage at the enamel and dentin margins.
Collapse